Описание материалов:
        
            Andur 8000 AP is a polyether (PPG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 80 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)].  Elastomers of lower hardness can be obtained by curing Andur 8000-AP with polyols and their combination with Curene 442 and other diamines, or through the use of plasticizers.
        
     
    
    
    | Физический | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Удельный вес  | 1.04 | g/cm³ | ASTM D792  | 
| Термокомплект | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Терморегулирующая вязкость  |  |  | ASTM D2393  | 
|     21°C  | 127000 | cP | ASTM D2393  | 
|     70°C  | 3400 | cP | ASTM D2393  | 
|     100°C  | 425 | cP | ASTM D2393  | 
| Дополнительная информация | 
|---|
| NCO: 3.3 to 3.7%Specific Gravity, ASTM D792, 70°F: 1.04 g/mlSpecific Gravity, ASTM D792, 212°F: 1.03 g/ml |