Описание материалов:
        
            KetaSpire® KT-820UFP is the low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-colored, ultra-fine powder form. This ultra-fine PEEK powder is suitable for water-borne coatings, electrostatically driven powder coatings and resin pre-impregnation of continuous fiber composites. This ultra-fine powder is produced to a median particle size D50 of about 10 micrometers.
KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent chemical resistance to acids, bases and a broad range of aggressive organic chemicals, best-in-class fatigue resistance, high thermal resistance, high purity and ease of melt processing.
These properties make KT-820UFP well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses.
The resin is also available in a natural-colored pellet form under the grade name KT-820 NT for injection molding and extrusion.
        
     
    
    
    | Главная Информация |  | 
|---|
| Характеристики  | - Хорошая стабильность размеров
 - Хорошая ударопрочность
 - Хорошая химическая стойкость
 - Сопротивление усталости
 - Теплостойкость, высокая
 - Пластичность
 - Огнестойкий
 
  | 
| Используется  | - Электрическое/электронное применение
 - Промышленное применение
 - Аэрокосмическое применение
 - Применение в автомобильной области
 - Поставки нефти/газа
 
  | 
| Соответствие RoHS  | - Свяжитесь с производителем
 
  | 
| Внешний вид  |  | 
| Формы  |  | 
| Метод обработки  | - Водное покрытие
 - Электростатическое распылительное покрытие
 
  | 
| Физический | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Удельный вес  | 1.30 | g/cm³ | ASTM D792  | 
| Поглощение воды (24 hr) | 0.10 | % | ASTM D570  | 
| Размер частиц  |  |  |   | 
|     D50  | 10.0 | µm |   | 
|     D90  | 16.0 | µm |   | 
|     D99  | 26.0 | µm |   | 
| Механические | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Модуль растяжения  | 3650 | MPa | ASTM D638  | 
| Прочность на растяжение  | 96.5 | MPa | ASTM D638  | 
| Удлинение при растяжении  |  |  | ASTM D638  | 
|     Yield  | 5.2 | % | ASTM D638  | 
|     Fracture 1 | 20 - 30 | % | ASTM D638  | 
| Флекторный модуль  | 3860 | MPa | ASTM D790  | 
| Flexural Strength  | 152 | MPa | ASTM D790  | 
| Воздействие | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Зубчатый изод Impact  | 69 | J/m | ASTM D256  | 
| Незубчатый изод Impact  | No Break |  | ASTM D256  | 
| Тепловой | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Температура отклонения при нагрузке (1.8 MPa, Unannealed) | 157 | °C | ASTM D648  | 
| Температура перехода стекла  | 150 | °C | ASTM D3417  | 
| Температура плавления  | 340 | °C | ASTM D3417  | 
| CLTE-
Поток (-50 to 50°C) | 4.3E-5 | cm/cm/°C | ASTM E831  | 
| Инструкции по впрыску | 
|---|
| Back Pressure: minimum | 
| Примечание | 
|---|
| 1 . | Tensile test speed = 2 in/min (50 mm/min) |