Описание материалов:
        
            Andur 70-DP is a polyether (PTMG) based liquid, toluene  diisocyanate terminated prepolymer. An elastomer with a hardness of 70 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)].  Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442 and other diamines, or by the use of plasticizers.
        
     
    
    
    | Физический | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Удельный вес  | 1.10 | g/cm³ | ASTM D792  | 
| Термокомплект | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Терморегулирующая вязкость  |  |  | ASTM D2393  | 
|     70°C  | 1060 | cP | ASTM D2393  | 
|     100°C  | 270 | cP | ASTM D2393  | 
| Дополнительная информация | 
|---|
| NCO: 8.8 to 9.2%Specific Gravity, ASTM D792, 77°F: 1.1 g/mlSpecific Gravity, ASTM D792, 212°F: 1.06 g/ml |