Andur 8 APFLM/Curene® 442
        
     
    
    
        Описание материалов:
        
            Andur 8-APF-LM is a polyester based liquid, toluene diisocyanate terminated prepolymer.  An elastomer with a hardness of 80 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)].  Elastomers of lower hardness can be obtained by curing Andur 8-APF-LM with polyols and their combination with Curene 442 and other diamines or by the use of plasticizers.  The short pot life of Andur 8-APF-LM makes it ideal for machine casting.
        
     
    
    
    | Главная Информация |  | 
|---|
| Характеристики  |  | 
| Формы  |  | 
| Физический | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Плотность  | 1.21 | g/cm³ | ASTM D1505  | 
| Формовочная усадка-
Поток  | 1.6 | % | ASTM D955  | 
| Твердость | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Твердость дюрометра (Shore D) | 80 |  | ASTM D2240  | 
| Эластомеры | Номинальное значение | Единица измерения | Метод испытания | 
|---|
| Tensile Stress  |  |  | ASTM D412  | 
|     100% strain  | 4.62 | MPa | ASTM D412  | 
|     300% strain  | 7.03 | MPa | ASTM D412  | 
| Прочность на растяжение (Yield) | 47.6 | MPa | ASTM D412  | 
| Удлинение при растяжении (Break) | 630 | % | ASTM D412  | 
| Комплект сжатия  | 26 | % | ASTM D395B  | 
| Сопротивляемость Bayshore  | 39 | % | ASTM D2632  | 
| Термокомплект | Номинальное значение | Единица измерения |  | 
|---|
| Срок службы горшка  | 5.0 - 6.0 | min |   | 
| Время демолд  | 30 | min |   | 
| Время доставки (96°C) | 16 | hr |   | 
| Дополнительная информация | 
|---|
| Durometer Hardness, ASTM D2240, Shore D: 78 to 82Die C Tear, ASTM D1004: 395 pliAverage Split Tear, ASTM D1938: 235 pliMix Temperature:
Andur 8 APLFM: 195-212°F
Curene 442: 235-250°F | 
| Инъекция | Номинальное значение | Единица измерения |  | 
|---|
| Температура формы  | 104 - 113 | °C |   |